Iron nickel alloy is obtained at a given temperature range by adjusting the content of nickel internal energy and the expansion coefficient of different soft glass and ceramic matching a series of expansion alloy, its expansion coefficient and the Curie temperature increases with the increase of nickel content.The assembly is widely used in electric vacuum industry the sealing structure of the material
Chemical Composition in %, Invar
brand | Chemical composition | ||||||||
Ni | Fe | C | P | Si | Co | Mn | Al | S | |
≤ | |||||||||
4j42 | 41.5~42.5 | Bal | 0.05 | 0.02 | 0.3 | - | 0.80 | 0.10 | 0.02 |
4j45 | 44.5~45.5 | Bal | 0.05 | 0.02 | 0.3 | - | 0.80 | 0.10 | 0.02 |
4j50 | 49.5~50.5 | Bal | 0.05 | 0.02 | 0.3 | 1.0 | 0.80 | 0.10 | 0.02 |
4j52 | 51.5~52.5 | Bal | 0.05 | 0.02 | 0.3 | - | 0.60 | - | 0.02 |
4j54 | 53.5~54.5 | Bal | 0.05 | 0.02 | 0.3 | - | 0.60 | - | 0.02 |
Basic physical constants and mechanical properties of the alloy:
brand | Thermal conductivity | Specific heat capacity | Density | Electric resistivity | Curie point |
4j52 | 16.7 | 502J | 8.25 | 0.43 | 520 |
Typical expansion character(10 -6 / ºC ) | ||||||||
Temperature range | 20~100 | 20~200 | 20~300 | 20~350 | 20~400 | 20~450 | 20~500 | 20~600 |
Expansion coefficient | 10.3 | 10.4 | 10.2 | 10.3 | 10.3 | 10.3 | 10.8 | 11.2 |
4 j52 alloy is mainly used for and soft lead glass sealing, small tube fuses.