Welcome to our websites!

Manufacture High Purty 99.6% Ni200 Ni201 Ni212 Pure Nickel N4 N6 Precision Stranded Alloy Wire for Power Tools Machinery

Short Description:


  • Model NO.: NI200,NI201, NI212
  • Density: 8.9 g/cm3
  • surface: bright
  • package: spool+Carton+ Case
  • trademark: TANKII
  • Origin: Shanghai China
  • Spool: DIN250,DIN200
  • HS Code: 75052200
  • Product Detail

    FAQ

    Product Tags

     

    Nickel Grade Ni+Co Cu Si Mn C Cr S Fe Mg
    Ni201 Bal. .25 .3 .35 .02 .2 .01 .3 -
    Ni200 Bal. .25 .3 .35 .15 .2 .01 .3 -

     

    Alloy

    Standard Strand Construction, mm

    Resistance,Ω/m

    Strand Diameter Nominal, mm

    Meter per Kilo

    NiCr 80/20

    18×0.544+1×0.574

    0.252-0.278

    2.67

    26

    NiCr 80/20

    19×0.61

    0.205-0.250

    3.05

     

    NiCr 80/20

    18×0.523+1×0.574

    0.271-0.299

    2.67

    30

    NiCr 80/20

    19×0.574

    0.227-0.251

    2.87

    25

    NiCr 80/20

    36×0.385+1×0.45

    0.265-0.293

    2.76

    26

    NiCr 60/15

    19×0.508

    0.286-0.318

    2.54

     

    NiCr 60/15

    18×0.523+1×0.574

    0.276-0.305

    2.76

    30

    Ni200/Ni201

    19×0.574

    0.019-0.021

    2.87

    21

     

     

    N6 Chromel C, Ni 60, N6, HAI-NiCr 60, Tophet C, Resistohm 60, Cronifer II,
    Electroloy, Nichrome, Alloy C, Ni  6, MWS-675, Stablohm 675
    N7 Ni 70, Chromel 70/30, N7, Hytemco, HAI-NiCr 70, Balco, Tophet 30,
    Resistohm 70, Cronix 70, Stablohm 710
    N8 Chromel A, Ni 80, N8, Nichrome V, HAI-NiCr 80, Tophet A, Resistohm
    80, Cronix 80, Protoloy, Ni  8, Alloy A, MWS-650, Stablohm 650

     

     

    Propertes/Grade Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30
    Main  Chemical  composition Ni Rest Rest 55.0-61.0 34.0-37.0 30.0-34.0
      Cr 20.0-23.0 28.0-31.0 15.0-18.0 18.0-21.0 18.0-21.0
      Fe ≤ 1.0 ≤ 1.0 Rest Rest Rest
    Max.  continuous  service  temp. of element 1200 1250 1150 1100 1100
    Resistivity  at  20oC  (μ Ω · m) 1.09 1.18 1.12 1.04 1.04
    Density  (g/cm3) 8.4 8.1 8.2 7.9 7.9
    Thermal  conductivity(KJ/m· h· oC) 60.3 45.2 45.2 43.8 43.8
    Coefficient  of  lines  expansion(α × 10-6/oC) 18 17 17 19 19
    Melting  point  (approx. )(  oC) 1400 1380 1390 1390 1390
    Elongation  at  rupture  (%) > 20 > 20 > 20 > 20 > 20
    Micrographic  structure austenite austenite austenite austenite austenite
    Magnetic  properties nonmagnetic nonmagnetic nonmagnetic nonmagnetic nonmagnetic

     

     

     

     

     

     

     

     

     